Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 103 MPa | 14900 psi | |
Poco Graphite AXZ-5Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
Compressive Strength | 103 MPa | 14900 psi | |
Pyrotek TS-235 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Tan color. Highly flexible. High heat resistance.Information provided by Pyrotek. |
|||
Compressive Strength | 103 MPa | 15000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Ertalyte® PET-P, Polyester-semi-crystalline thermoplastic, extruded (ASTM Product Data Sheet) |
|||
Compressive Strength | 103 MPa | 15000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near .. |
|||
Compressive Strength | 103 MPa | 15000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Techtron® PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded (ASTM Product Data Sheet) |
|||
Compressive Strength | 103 MPa | 15000 psi | Ultimate; TM R050-38 |
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where .. |
|||
Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
Technetics Group Amicon™ PET-P
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
Quantum PET Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Strength | 103 MPa | 14900 psi | |
Haysite 18600 Polyester BMC, 15% Glass Reinforced The 18600 series bulk molding compound can be compression, transfer, or injection molded. Formulated with a high temperature resin system, this grade exhibits exceptional retention of physical and e.. |
|||
Compressive Strength | 103 MPa | 14900 psi | |
Haysite 30000 Polyester BMC, 15% Glass Reinforced Haysite 30000 series bulk molding compound is a general purpose material. This compound can be compression, transfer, or injection molded. This material has good mechanical properties and can be pig.. |
|||
Compressive Strength | 103 MPa | 14900 psi | |
Haysite 43000 Polyester SMC, 22% Glass Reinforced The 43000 series sheet molding compound is a general purpose material. Designed for compression molding, this grade exhibits good mechanical properties and resistance to mild corrosive agents. |
|||
Compressive Strength | 103 MPa | 14900 psi | |
Haysite 48600 Polyester SMC, 30% Glass Reinforced The 48600 series sheet molding compound is formulated with a high temperature resin system (180º C). Designed for compression molding, this grade offers excellent retention of physical and electr.. |
|||
Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
Techmer ES Plaslube® J-1850/30/TF/15 PBT, 30% GFR, 15% PTFE |
|||
Compressive Strength | >= 103 MPa | >= 15000 psi | |
Master Bond EP21SC-1 Two Component Epoxy Resin System Product Description: Master Bond Polymer System EP21SC-1 is a two component epoxy system featuring abrasion resistance. This high performance compound utilizes silicon carbide as a filler material a.. |
|||
Compressive Strength | >= 103 MPa | >= 15000 psi | |
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy Description: Master Bond EP30AN-1 is a two part epoxy for high performance potting, sealing, coating and bonding featuring high thermal conductivity, excellent electrical insulation properties and N.. |
|||
Compressive Strength | 103 MPa @Time 360000 sec |
14900 psi @Time 100 hour |
|
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Compressive Strength | 103 MPa | 14900 psi | DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Compressive Strength | >= 103 MPa | >= 14900 psi | Ambient |
China-Yixing Longly Refractories Push Slab Corundum-Mullite Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine.. |
|||
Compressive Strength | 103 MPa | 15000 psi | |
3M Scotchkote™ EG 513 Epoxy Ceramic Rebuild Scotchkote Epoxy Ceramic Repair EG 513 has been specifically developed as a ceramic filled repair system for rebuilding and repairing equipment requiring good mechanical strength, combined with abra.. |
|||
Compressive Strength | 103 MPa | 15000 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced FR Polyester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Compressive Strength | 103 MPa | 15000 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Compressive Strength | 103 MPa | 15000 psi | Crosswise; ASTM D635 |
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Compressive Strength | 103 - 117 MPa | 15000 - 17000 psi | |
Bulk Molding Compounds BMC 1401 Encapsulating Material, Electrical Grade BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for co.. |
|||
Compressive Strength | 103 - 131 MPa | 15000 - 19000 psi | |
Bulk Molding Compounds BMC A20-(a) High Strength Grade Molding Compound BMC A20 is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A20 is well suited for injection, transfer or compression molding o.. |
|||
Compressive Strength | 103 MPa | 15000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Nylatron® MC® 907 Natural Nylon, Monocast® FDA Compliant, Unfilled Type 6 (ASTM Product Data Sheet) |
|||
Compressive Strength | 103 MPa | 15000 psi | ASTM D695 |
Technetics Group Amicon™ Acetal Copolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Compressive Strength | 103 MPa | 15000 psi | Break; TM R050-38 |
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th.. |
|||
Compressive Strength | 103 - 138 MPa | 15000 - 20000 psi | |
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi.. |