Polymer Property : Compressive Strength = 10300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 71.0 MPa
10300 psi
Pyrotek NAD-1000 High Temperature Engineering Board
NAD-1000 is a high density calcium silicate board reinforced with selected fibers to produce excellent thermal characteristics and dimensional stability up to 1000°C. NAD-1000 retains high strengt..
Compressive Strength 71.0 MPa
10300 psi
Elastic Limit
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis..
Compressive Strength 71.0 MPa
10300 psi
ultimate load
BNZ Materials CS85 High Temperature Structural Insulation
NZ manufactures a variety of non-asbestos calcium silicate structural insulations that combine high strength and excellent thermal insulating characteristics for use in a variety of heat processing,..
Compressive Strength 71.0 MPa
10300 psi
for Epoxy Coating
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
Compressive Strength 71.0 - 98.6 MPa
10300 - 14300 psi
Bulk Molding Compounds BMC HT12-1024 Automotive Grade Molding compound
BMC HT12-1024 is a high temp wear resistant molding compound designed for automotive brush holders. It is listed under Ford WS-MSD-A. It can be injection or transfer molded.Information provided by..