Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
PolyOne LubriOne™ NY-10GF/10T BLACK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Compressive Strength | 96.5 MPa | 14000 psi | |
Poco Graphite EDM-200 EDM Graphite POCO's EDM-200 is an isotropic Superfine particle graphite providing good strength, surface finish, and wear resistance.Applications:Structural ribsRoughing or finishing electrodesLarge featured mol.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series A-100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series A-130 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0040 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0070 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0100 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0140 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series P-0230 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series Premium 5MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series Glass Spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet) |
|||
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
Quantum PPSU Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Strength | 96.5 MPa | 14000 psi | |
Resin Technology Group KONA 877 Low Viscosity, Low Shrinkage, Vacuum Grade Casting Resin Mix ratio 1 to 1 by weight.KONA 877 with HARDENER #112 is a versatile epoxy casting system developed for high performance production potting and encapsulating applications where low shrinkage and ra.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Break; TM R050-38 |
Resinlab® EP1325LV Thixotropic, Heat Curing Epoxy Adhesive Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where .. |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series Premium 2MM Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | ASTM D695 |
Techmer ES Luriblend® PA6 E ML2 MB Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | 10% strain; ASTM D695 |
Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Compressive Strength | >= 96.5 MPa | >= 14000 psi | |
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System Product Description: Master Bond Polymer Adhesive EP21AOLV-1 is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant and coating. This versatile system will adhere t.. |
|||
Compressive Strength | >= 96.5 MPa | >= 14000 psi | |
Master Bond EP30ND Non-Drip, Dimensionally Stable Epoxy Adhesive Description: Master Bond Polymer System EP30ND is a high viscosity, two component epoxy adhesive/sealant with a paste consistency. It will cure at room temperature or more rapidly at elevated temper.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | cured |
Atom Adhesives AA-DUCT 902LP Epoxy Adhesive AA-DUCT 902LP is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value .. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | cured |
Atom Adhesives AA-DUCT 903 Epoxy Adhesive AA-DUCT 903 is an epoxy adhesive and coating formulation based on Nickel. This epoxy nickel formulation offers the maximum continuity of conductivity with an electrical resistivity value of less tha.. |
|||
Compressive Strength | 96.5 - 124 MPa | 14000 - 18000 psi | |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Quadrant CPVC - ASTM D1748, Cell Classification (ASTM Product Data Sheet) |
|||
Compressive Strength | 96.5 - 248 MPa | 14000 - 36000 psi | |
Potters Industries A-Series A-120 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Break; TM R050-38 |
Resinlab® EP1046FG Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Black is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Ultimate; TM R050-38 |
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Compressive Strength | 96.5 MPa | 14000 psi | Break; TM R050-38 |
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Compressive Strength | 96.6 MPa | 14000 psi | |
Henkel Hysol EA 9395 Paste Adhesive System Two-part, nonmetallic-filled version of Hysol EA 9394.Applications: Potting Structural Repair Composite Bonding |