Compressive Strength 142.96 MPa
20735 psi
5% Def.; ISO 604
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet)
KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re..