Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer Quadrant Engineering Plastics Products
Trade Name Ketron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. The composition of the Invibio PEEK-CLASSIX White resin complies with the regulations that apply in the Member States of the European Union (Directive 2002/72/EC, as amended) and in the United States of America (FDA) for plastic materials and articles intended to come into contact with foodstuffs. KETRON PEEK-CLASSIX LSG stock shapes have also been successfully type tested for their compliance with both United States Pharmacopeia (USP) and ISO 10993-1 guideline requirements for Biocompatibility Testing of Materials, and they come with full traceability from resin to stock shape. These features, added to an excellent sterilizability by means of steam, dry heat, ethylene oxide, plasma and gamma irradiation, make KETRON PEEK-CLASSIX LSG stock shapes very suitable for applications in the medical, pharmaceutical and biotechnology markets. Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Water Absorption 0.050 %
0.050 %
Immersion, 24hr; ISO 62
0.11 %
0.11 %
Immersion, 96hr; ISO 62
Moisture Absorption at Equilibrium 0.20 %
0.20 %
23°C/50% R.H.
Water Absorption at Saturation 0.45 %
0.45 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 105
105
ISO 2039-2
Ball Indentation Hardness 190 MPa
27600 psi
ISO 2039-1
Tensile Strength 114.97 MPa
16675 psi
ASTM D638
Tensile Strength, Yield 115 MPa
16700 psi
ISO 527
Elongation at Break 14 %
14 %
ISO 527
Elongation at Yield 4.5 %
4.5 %
ISO 527
Tensile Modulus 4.34 GPa
630 ksi
ASTM D638
Flexural Strength 172 MPa
25000 psi
ASTM D790
Compressive Strength 40.0 MPa
5800 psi
10% Def.; ASTM D695
79.01 MPa
11460 psi
2% Def.; ISO 604
142.96 MPa
20735 psi
5% Def.; ISO 604
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Charpy Impact Unnotched 40.0 J/cm²
190 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179-1/1eA
K (wear) Factor 755 x 10-8 mm³/N-M
375 x 10-10 in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 0.298 MPa-m/sec
8500 psi-ft/min
4:1 safety factor; QTM 55007
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 23.0 - 100 °C
27.8 µin/in-°F

@Temperature 73.4 - 212 °F
ASTM E831
55.1 µm/m-°C

@Temperature 23.0 - 150 °C
30.6 µin/in-°F

@Temperature 73.4 - 302 °F
ASTM E831
130 µm/m-°C

@Temperature >=150 °C
72.2 µin/in-°F

@Temperature >=302 °F
ASTM E831
Thermal Conductivity 0.251 W/m-K
1.74 BTU-in/hr-ft²-°F
Melting Point 340 °C
644 °F
ISO 11357
Maximum Service Temperature, Air 250 °C
482 °F
Long Term
310 °C
590 °F
Short Periods
Deflection Temperature at 1.8 MPa (264 psi) 165 °C
329 °F
ISO 75
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 35 %
35 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
IEC 60093
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI Yes
Yes
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Limited
Limited
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Descriptive Properties Value Comments
Color Natural