Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 97.9 MPa | 14200 psi | |
Poco Graphite EDM-1 EDM Graphite Applications:Fabricating electrodes with good detail Low wear electrodes High detail roughing electrodesMolds and dies |
|||
Compressive Strength | 97.9 MPa | 14200 psi | |
Poco Graphite PYROGRAPH Ion Implant Grade Graphite Pyrograph is pyrolytically infiltrated graphite. POCO's proprietary process infiltrates the base material to a minimum depth of 0.1 inch throughout the entire surface of the component. This process .. |
|||
Compressive Strength | 97.9 MPa | 14200 psi | |
Engineered Syntactic Systems AZ-40 Deep Water Syntactic Foam Syntactic foams are a combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high c.. |
|||
Compressive Strength | 97.9 MPa | 14200 psi | ASTM C579 |
Chesterton ARC 988 Composite Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physi.. |
|||
Compressive Strength | 98.1 MPa | 14200 psi | Cold Crushing Strength |
Chosun Refractories AC-2 Acid-Proof and Heat-Resistant Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 98.1 MPa | <= 14200 psi | Cold Crushing Strength |
Chosun Refractories CUN-718 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 98.1 MPa | <= 14200 psi | Cold Crushing Strength |
Chosun Refractories CUN-810 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 98.1 MPa | <= 14200 psi | Cold Crushing Strength |
Chosun Refractories CUN-846 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 98.1 MPa | <= 14200 psi | Cold Crushing Strength |
Chosun Refractories CUN-941 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 98.1 MPa | <= 14200 psi | Cold Crushing Strength |
Chosun Refractories CUN-B817 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 98.1 MPa | 14200 psi | Cold Crushing Strength |
Chosun Refractories Filter Dam Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 98.1 MPa | 14200 psi | Cold Crushing Strength |
Chosun Refractories KSB-A85 Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 98.1 MPa | 14200 psi | Cold Crushing Strength |
Chosun Refractories SAL85BR Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 98.1 MPa | 14200 psi | Cold Crushing Strength |
Chosun Refractories SAL90C Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 98.1 MPa | 14200 psi | Cold Crushing Strength |
Chosun Refractories SAL95 Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 98.1 MPa | 14200 psi | Cold Crushing Strength |
Chosun Refractories SB75 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 98.1 MPa | 14200 psi | Cold Crushing Strength |
Chosun Refractories SB-C Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 98.1 MPa | 14200 psi | Cold Crushing Strength |
Chosun Refractories SF-S Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 98.1 MPa | 14200 psi | Cold Crushing Strength |
Chosun Refractories ZR-C Special brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 98.1 MPa | <= 14200 psi | Cold Crushing Strength |
Chosun Refractories CSN-A114 Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 98.1 MPa | <= 14200 psi | Cold Crushing Strength |
Chosun Refractories CSN-A116 Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |