Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1500 - 2200 MPa | 218000 - 319000 psi | Crushing Strength |
China-Yixing Longly Refractories Alumina Grinding Balls and Lining Bricks Microcrystal Wear-Resistant Alumina Grinding Media (Balls) and Lining Bricks Characteristics: LONGLY adopts isostatic pressing and dry pressing in the forming process. We provide a variety of products with different dimension and specification. These products are extremely.. |