Polymer Property : Compressive Strength = 218000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1500 - 2200 MPa
218000 - 319000 psi
Crushing Strength
China-Yixing Longly Refractories Alumina Grinding Balls and Lining Bricks Microcrystal Wear-Resistant Alumina Grinding Media (Balls) and Lining Bricks
Characteristics: LONGLY adopts isostatic pressing and dry pressing in the forming process. We provide a variety of products with different dimension and specification. These products are extremely..