Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.22 MPa | 177 psi | 20 g/l |
Jackon JACKOCELL® R211 Expanded Polystyrene Construction and Block Molding High quality processingHigh strengthLow wasteFast moulding cycles |
|||
Compressive Strength | 1.22 MPa | 177 psi | 20 g/l |
Jackon JACKOCELL® R212 Expanded Polystyrene Construction and Block Molding High quality processingHigh strengthLow wasteFast moulding cycles |
|||
Compressive Strength | 1.22 MPa | 177 psi | 20 g/l |
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a.. |