Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.127 MPa | 18.5 psi | 48 hour silo aging time, 20 kg/m^3 |
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |