Compressive Strength 1240 MPa
180000 psi
Meehanite GA-50 Flake Graphite Cast Iron
Type GA-50 combines high strength, toughness, wear resistance and damping capacity with excellent machinability. Responds well to heat treatment, local and surface hardening.General Meehanite infor..