Mechanical Properties Metric English Comments
Compressive Strength 1.27 MPa
184 psi
48 hour silo aging time, 20 kg/m^3
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ..
Compressive Strength 1.27 MPa
184 psi
50 g/l
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be..