Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 130 - 140 MPa | 18900 - 20300 psi | ISO 604 |
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati.. |