Mechanical Properties Metric English Comments
Compressive Strength 242 MPa
35100 psi
ISO 604
Vyncolit A2710 Glass Fiber Reinforced Novolac Phenolic
Vyncolit® A2710 is a glass fiber reinforced phenolic molding compound with excellent mechanical and thermal properties.Information provided by Sumitomo Bakelite North America, Inc.
Compressive Strength 242 MPa
35100 psi
ASTM D695
Sumitomo Bakelite North America Epiall® 1960B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Epiall 1960B-1 is a mineral and short fiberglass filled epoxy compound, formulated for the encapsulation of passive electronic devices.Information provided by Sumitomo Bakelite North America, Inc.