Mechanical Properties Metric English Comments
Compressive Strength 3100 MPa
450000 psi
HRC 62 R<sub>m</sub>
Assab Steels ASSAB XW-42 Cold Work Steel
XW-42 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength High hardness after hardeningGood through-hardeni..