Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 3100 MPa | 450000 psi | HRC 62 R<sub>m</sub> |
Assab Steels ASSAB XW-42 Cold Work Steel XW-42 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength High hardness after hardeningGood through-hardeni.. |