Compressive Strength 228 MPa
33100 psi
ASTM D-695
Glastic 1120 Corrosion-Resistant Panels
Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1120 is an asbestos..
Compressive Strength 228 MPa
33100 psi
ASTM D695
Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate
Data provided by Glastic Corporation.NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern.
Compressive Strength 228 MPa
33100 psi
Haysite HST-II Glass Reinforced Polyester Sheet, Electrical Grade
UL, Inc. has granted HST-II the highest thermal recognition ever achieved by any glass polyester laminate (U.L. File No. E81893). HST-II has a 220º C/210º C rating for 1/8" thick and heavier,..