Material Notes:
Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1120 is an asbestos-free fiberglass-reinforced thermoset resin sheet. This material has very low water absorption and also has good splash and spill resistance to acids, weak bases and aliphatic hydrocarbons. Grade 1120 is UL classified, has high strength, and has a bright white finish(no painting necessary). Applications include fume hood liners, chemical storage cabinets and wall surfaces.Information provided by Glastic Corporation
Physical Properties Metric English Comments
Specific Gravity 1.81 g/cc
1.81 g/cc
ASTM D-792
Water Absorption 0.40 %
0.40 %
% by wt.; ASTM D-570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.8 MPa
7800 psi
ASTM D-638
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D-638
Flexural Strength 152 MPa
22100 psi
ASTM D-790
90.3 MPa

@Temperature 130 °C
13100 psi

@Temperature 266 °F
ASTM D-790
Compressive Strength 228 MPa
33100 psi
ASTM D-695
Izod Impact, Notched 4.75 J/cm
8.90 ft-lb/in
ASTM D-256
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Thermal Conductivity 0.270 W/m-K
1.87 BTU-in/hr-ft²-°F
ASTM C-177
Flame Spread Index 15
15
United States Calculation; ASTM E-84
20
20
Canadian Calculation; ASTM E-84
Descriptive Properties Value Comments
Smoke Developed over 500
ASTM E-84
Standard Color White
UL Recognition File Number R9599