Polymer Property : Compressive Strength = 38900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 268 MPa

@Temperature 23.0 °C
38900 psi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT™ 2021 Polyimide, 15% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Compressive Strength 268 MPa
38900 psi
ASTM D-695
Glastic GLASGUARD Scuff and Bulkhead Liners
GlasGuard Scuff and Bulkhead Liners serve as a method of protecting trailer walls from damage caused by forklift trucks and careless loading and unloading of freight. Manufactured of 1/4" thick fib..