Glastic GLASGUARD Scuff and Bulkhead Liners

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS
Manufacturer Glastic
Trade Name GLASGUARD
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Glastic GLASGUARD Scuff and Bulkhead Liners.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GlasGuard Scuff and Bulkhead Liners serve as a method of protecting trailer walls from damage caused by forklift trucks and careless loading and unloading of freight. Manufactured of 1/4" thick fiberglass-reinforced plastic (FRP). Offers lasting durability, no jagged edges, corrosion, rust, and moisture absorption resistance, weighs less, costs less, and fits flat. USDA approved.Information provided by Glastic Corporation
Physical Properties Metric English Comments
Specific Gravity 1.78 g/cc
1.78 g/cc
ASTM D-792
Water Absorption 0.30 %
0.30 %
% by wt.; ASTM D-570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 98.53 MPa
14290 psi
ASTM D-638
Tensile Modulus 12.6 GPa
1830 ksi
ASTM D-638
Flexural Strength 150.1 MPa
21770 psi
ASTM D-790
Flexural Modulus 12.1 GPa
1760 ksi
ASTM D-790
Compressive Strength 268 MPa
38900 psi
ASTM D-695
Shear Strength 92.4 MPa
13400 psi
ASTM D-732
Izod Impact, Notched 5.23 J/cm
9.80 ft-lb/in
ASTM D-256
Thermal Properties Metric English Comments
CTE, linear 22.0 µm/m-°C

@Temperature 20.0 °C
12.2 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Thermal Conductivity 0.260 W/m-K
1.80 BTU-in/hr-ft²-°F
ASTM C-177
Descriptive Properties Value Comments
Standard Color White
Users viewing this material also viewed the following: