Mechanical Properties Metric English Comments
Compressive Strength 280 - 330 MPa
40600 - 47900 psi
ISO 604
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
Compressive Strength 280 MPa
40600 psi
ASTM D695
Sumitomo Bakelite North America E 8398 Hardware Grade Epoxy
Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Vyncolit, a Sumitomo B..
Compressive Strength 280 MPa
40600 psi
ISO 604
Vyncolit X680 Novolac Phenolic
Glass fiber and glass bead filled phenolic molding compound with excellent mechanical and thermal properties. Easily transformed into complex shapes. UL listed.USES: Complex precision parts with t..
Compressive Strength 280 MPa
40600 psi
ISO 604
Vyncolit X6952 Novolac Phenolic
Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn..
Compressive Strength 280 MPa

@Thickness >=5.00 mm
40600 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Sheets
Description: Reinforced with a finer cotton fabric than Etronax MF. Also well suited in particular for small components which are subject to mechanical load and wear. Can be machined to finer tolera..
Compressive Strength 280 MPa

@Thickness >=5.00 mm
40600 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola Etronax MMMF Phenolic, Cotton Fabric Reinforcement, Light Brown, Sheets
Description: Friction reducing material consisting of phenolic resin and a very fine cotton fabric. Exclusively for mechanical applications. Good dry-run properties but can be lubricated with oil, g..
Compressive Strength 280 MPa

@Treatment Temp. 50.0 °C,
Time 3600 sec
40600 psi

@Treatment Temp. 122 °F,
Time 1.00 hour
ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m..