Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 434 MPa @Temperature 21.1 °C |
63000 psi @Temperature 70.0 °F |
Dry; Vacuum/Oven Cured; SACMA 1-94 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Compressive Strength | 434 MPa | 63000 psi | ASTM D695 |
G-11 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Compressive Strength | 434 MPa @Thickness 12.7 mm |
63000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP511 Glass Fabric Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat.. |
|||
Compressive Strength | 434 MPa | 62900 psi | ISO 604 |
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperaturesInformation provided by Sumitomo Bak.. |
|||
Compressive Strength | 434 MPa @Temperature 20.0 °C |
62900 psi @Temperature 68.0 °F |
|
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |