Compressive Strength 34.3 MPa
4980 psi
Cold Crushing
Sharadaa Ceramics KYANITE Mullite
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 34.3 MPa
4980 psi
Cold Crushing
Sharadaa Ceramics LI 50K High Alumina Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 34.3 MPa

@Temperature 110 °C
4980 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFCAST SUPER Dense Castables
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 34.3 MPa
4980 psi
Cold Crushing Strength
Chosun Refractories CRAG-S81 Long Stopper
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 34.3 MPa
4980 psi
Cold Crushing Strength
Chosun Refractories N1-2 Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 34.3 MPa
4980 psi
Cold Crushing Strength
Chosun Refractories N2-1 Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 34.3 MPa
4980 psi
Cold Crushing Strength
Chosun Refractories N3-1 Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 34.3 MPa
4980 psi
Cold Crushing Strength
Chosun Refractories CH-3 Hard Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 34.3 MPa
4980 psi
Cold Crushing Strength
Chosun Refractories N4-1 Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 34.3 MPa
4980 psi
Cold Crushing Strength
Chosun Refractories N5 Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 34.3 MPa
4980 psi
BCC Products HPX-850 Epoxy Backfill System
HPX-850 is a light weight, heat resistant, two component epoxy backfill system. HPX-850 features advantages such as low cost, long pot life, machineability, and low shrinkage. HPX-850 is ideally su..