Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories CRAG-S81 Long Stopper

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CRAG-S81 Long Stopper.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.75 g/cc
0.0994 lb/in³
Porosity 16.3 %
16.3 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.008829 GPa

@Temperature 1400 °C
1.281 ksi

@Temperature 2550 °F
0.00981 GPa

@Temperature 23.0 °C
1.42 ksi

@Temperature 73.4 °F
Compressive Strength 34.3 MPa
4980 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 4.30 µm/m-°C

@Temperature 1000 °C
2.39 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 80 %
80 %
Descriptive Properties Value Comments
Chemical Analysis(%),FC+SiC 16+2
Remarks For erosive steel
Users viewing this material also viewed the following: