Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 50.4 MPa | 7310 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed.. |