Mechanical Properties Metric English Comments
Compressive Strength 35.0 MPa
5080 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Omnia Plastica PPS GF40 Polyphenylenesulphide
Crystalline polymer based on polyphenylene sulfide with the addition of 40% glass-fibre. Very high rigidity, stiffness and flexural strength. The temperature resistance is very high: up to 240° C. ..
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Gouda Vuurvast A Vuurvast Dense Refractory Brick
Description: A general purpose high quality fireclay brick for use up to 1400°C. Reasonably good thermal shock resistance.Remarks: This data represents average values, obtained from samples that ..
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Gouda Vuurvast B 1 Dense Refractory Brick
Description: B 1 is a fireclay quality for general applications up to 1350°CRemarks: This data represents average values, obtained from samples that were cut from standard bricks.Information prov..
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Gouda Vuurvast C Dense Refractory Brick
Description: A dry-pressed fireclay brick for use up to 1250°C with a good resistance to acid slags and vapors. Application: industrial furnaces, chimneys, electrolytic reduction cells.Remarks: T..
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Gouda Vuurvast B Dense Refractory Brick
Description: A dry-pressed fireclay brick for use up to 1300°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda..
Compressive Strength 35.0 MPa

@Time 3.60e+7 sec
5080 psi

@Time 10000 hour
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified
Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Chosun Refractories A18H Magnesia Carbon Bricks for Electric Arc Furnace
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Chosun Refractories A18HM Magnesia Carbon Bricks for Electric Arc Furnace
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Chosun Refractories A18S Magnesia Carbon Bricks for Electric Arc Furnace
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Chosun Refractories C18A Magnesia Carbon Brick for Converter
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Chosun Refractories C18B Magnesia Carbon Brick for Converter
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Chosun Refractories C18C Magnesia Carbon Brick for Converter
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Chosun Refractories C18CX Magnesia Carbon Brick for Converter
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Chosun Refractories C18D Magnesia Carbon Brick for Converter
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Chosun Refractories C18DX Magnesia Carbon Brick for Converter
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength >= 35.0 MPa
>= 5080 psi
Ambient
China-Yixing Longly Refractories ASM-120 Cordierite-Mullite
Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b..
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Chosun Refractories C18AX Magnesia Carbon Brick for Converter
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).