Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast C Dense Refractory Brick

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast C Dense Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A dry-pressed fireclay brick for use up to 1250°C with a good resistance to acid slags and vapors. Application: industrial furnaces, chimneys, electrolytic reduction cells.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 1.95 g/cc
0.0704 lb/in³
Apparent
Porosity 20 %
20 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 35.0 MPa
5080 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.950 W/m-K

@Temperature 100 °C
6.59 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.10 W/m-K

@Temperature 650 °C
7.63 BTU-in/hr-ft²-°F

@Temperature 1200 °F
1.20 W/m-K

@Temperature 1100 °C
8.33 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Maximum Service Temperature, Air 1250 °C
2280 °F
1275 °C
2327 °F
Deformation under load - t<sub>a</sub>
Component Elements Properties Metric English Comments
Al2O3 25 - 28 %
25 - 28 %
Fe2O3 2.0 %
2.0 %
SiO2 65 - 66 %
65 - 66 %
Descriptive Properties Value Comments
Segercone 28-29
Thermal Shock Resistance 5 cycles
DIN 51068