Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 40.5 MPa @Strain 3.50 % |
5870 psi @Strain 3.50 % |
DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-530KF15 A5M Polymer Alloy Main Characteristics: High elongation; High impact strength; Stress resistantApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInformation provided by Zed.. |