Mechanical Properties Metric English Comments
Compressive Strength 0.0420 MPa
6.09 psi
Resistance at 10%, 350 kg/m³; ASTM C165
Microtherm Group Molded Pipe Sections Filament Reinforced Silica Pipe Insulation
Microtherm® Moulded Pipe Sections (MPS) are preformed pieces of pipe insulation designed to provide a thermally efficient insulation system for piping of all sizes from 25 mm (1”) upwards. F..