Polymer Property : Compressive Strength = 63.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 63.7 MPa
9250 psi
Cold Crushing Strength
Chosun Refractories SAL60 Special Alumina brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 63.7 MPa
9250 psi
Cold Crushing Strength
Chosun Refractories SF34 Hard Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 63.7 MPa
9250 psi
Cold Crushing Strength
Chosun Refractories CER-80 Special Casting Block
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).