Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories SF34 Hard Fireclay brick

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SF34 Hard Fireclay brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.32 g/cc
0.0838 lb/in³
Porosity 15 %
15 %
Mechanical Properties Metric English Comments
Compressive Strength 63.7 MPa
9250 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 5.60 µm/m-°C

@Temperature 1000 °C
3.11 µin/in-°F

@Temperature 1830 °F
Shrinkage -0.200 - 0.20 %

@Temperature 1500 °C,
Time 7200 sec
-0.200 - 0.20 %

@Temperature 2730 °F,
Time 2.00 hour
Component Elements Properties Metric English Comments
Al2O3 43 %
43 %
Fe2O3 1.2 %
1.2 %
Descriptive Properties Value Comments
Quality Anti-abrasion, Anti-spalling, Anti-corrosion
Refractories Under Load(2kg/?,T2?) 1,500
Refractoriness (SK) 34
Users viewing this material also viewed the following: