Mechanical Properties Metric English Comments
Compressive Strength 72.4 MPa
10500 psi
ASTM D695
Quantum PVDF
Information provided by Quantum Advanced Engineering Plastics
Compressive Strength 72.4 MPa
10500 psi
ASTM D695
Quantum PBT
Information provided by Quantum Advanced Engineering Plastics