Mechanical Properties Metric English Comments
Compressive Strength 55.2 MPa
8000 psi
ASTM D695
Plaskolite Vivak PETG Sheet
VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details...
Compressive Strength 55.2 MPa
8000 psi
Break; Mixed 2:1; TM R050-38
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
Compressive Strength 55.2 MPa
8000 psi
Ultimate; Mixed 2:1; TM R050-38
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
Compressive Strength 55.2 MPa
8000 psi
Break; TM R050-38
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
Compressive Strength 55.16 - 82.74 MPa
8000 - 12000 psi
after 816°C
Pyrotek Pyrocast ZEAL Refractory Shapes
Aggregate Base: MulliteApplicationsDoor sill Furnace ramp Crucible bottom / lining Information provided by Pyrotek.
Compressive Strength >= 55.2 MPa
>= 8000 psi
Master Bond EP38CL Adhesive Features Toughness and Durability
Description: Master Bond EP38CL is a lower viscosity, optically clear two component epoxy system for high performance bonding, coating, sealing and small encapsulations, featuring toughness and dura..
Compressive Strength 55.2 MPa
8000 psi
CMT Materials HYTAC® C Castable Syntactic Tooling
HYTAC-C is a one-part castable product in the HYTAC family of syntactics. This product is available as an uncured, single component mixture that may be poured or cast into a wide variety of shapes a..
Compressive Strength 55.2 MPa
8000 psi
3M HGS8000X Glass Bubbles
3M™ Glass Bubbles HGS Series are engineered hollow glass spheres for use as a density reducing agent for oil and gas drilling fluids and drilling cements. The spherical shape of 3M glass bubbles of..
Compressive Strength 55.2 MPa
8000 psi
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina
Coarse grain castable for producing large hi-temp tooling.
Compressive Strength 55.2 MPa
8000 psi
Aremco Ceramacast™ 586 High Temperature Potting & Casting Material Zirconia Silicate
Castable ceramic for ceramic and metal assemblies. Excellent handling, fast curing.
Compressive Strength 55.2 MPa
8000 psi
Aremco Ceramacast™ 900 High Temperature Potting & Casting Material Zirconia Silicate
High Density, high strength molding compound.
Compressive Strength 55.2 - 110 MPa
8000 - 16000 psi
Compared to 3500 for concrete
Abatron AboJet Structural Crack-Injection Resin
Structural crack injection resin for foundations, dikes, columns, load-bearing walls and structures. Offers strength, performance, durability, cost effectiveness and restoration instead of demoliti..
Compressive Strength 55.2 MPa
8000 psi
perpendicular
Carlisle 201HL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Compressive Strength 55.2 MPa
8000 psi
10% Def.; ASTM D695
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet)
Compressive Strength 55.2 MPa
8000 psi
Ultimate; TM R050-38
Resinlab® EP1296 Highly Filled, Moderately Thixotropic Black Casting Resin
Resinlab™ EP1296 is a highly filled, moderately thixotropic black casting resin designed for applications requiring good thermal conductivity, low shrinkage and a low CTE. It was especially formula..
Compressive Strength >= 55.2 MPa
>= 8000 psi
Master Bond EP30M4LV Chemically Resistant, Low Viscosity Adhesive
Description: Master Bond EP30M4LV is a two component, low viscosity epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weig..