Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 572 MPa @Temperature 23.9 °C |
83000 psi @Temperature 75.0 °F |
Dry; Oven Cure 275°F, 90 min; ASTM D695 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K 2x2 Twill Carbon Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Compressive Strength | 572 MPa | 83000 psi | ASTM D695 |
Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber Greene Tweed offers precision-molded thermoplastic components made from our high-performance Orthtek® composite materials for a variety of demanding medical and biotechnology applications. Ortht.. |
|||
Compressive Strength | 572 MPa | 83000 psi | ASTM D695 |
Greene Tweed WR™ 575 PEEK, Bi-Directional Carbon Fiber Filled WR®575 is a thermoplastic composite consisting of bi-directionally oriented carbon fibers in a PEEK matrix. The excellent wear resistance and the fiber orientation of WR575 makes this material i.. |