Mechanical Properties Metric English Comments
Compressive Strength 6.00 MPa
870 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Omnia Plastica Akulon® PA6 G.Oil - Omniamid Oil - at 50% RH
Cast Nylon 6 with the addition of 6% of special lubricating oil which remains in solution in the material. The unique method of production results in a micro distribution of oil particles with a hom..
Compressive Strength 6.00 MPa
870 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Omnia Plastica Omniamid PA 6 - Akulon 6 - at 50% RH
Semi-crystalline polymer of polyamide obtained by the polymerisation of the caprolactam. Its large popularity is due to both its good overall features as well as its cost-performance relationship. T..
Compressive Strength 6.00 MPa
870 psi
1% strain over 1000 hours; ISO.899 DIN.53444
Omnia Plastica Omniamid PA6 GHR - HR - at 50% RH
Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i..
Compressive Strength 6.00 MPa
870 psi
Solid; ASTM D1621
Sawbones Fourth-Generation Simulated Cancellous Bone (Rigid Polyurethane Bone)
Fourth-generation bones model natural cortical bone using a mixture of short glass fibers and epoxy resin pressure injected around a foam core. Standard bone models are manufactured with a solid rig..
Compressive Strength 6.00 MPa

@Strain 3.50 %
870 psi

@Strain 3.50 %
DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-100EL55 A1F Polymer Alloy, Elastomer Modified
Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol..
Compressive Strength 6.00 MPa
870 psi
In the In Plane Direction
Cymat A35620SC 040SS Stabilized Aluminum Foam
Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it ..