Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 965 MPa | 140000 psi | |
Performance Alloys MoldStar® 90 Copper Mold Alloy Description: MoldStar® 90 is a beryllium-free copper alloy for the blow molding and injection molding industries as well as other industrial applications. MoldStar® 90 provides a good balance of t.. |