Polymer Property : Compressive Strength = 9800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 67.6 MPa
9800 psi
ASTM D695
Greene Tweed ARâ„¢ HT Abrasive-Resistant Thermoplastic
ARHT™ is a proprietary thermoplastic material specifically developed for use a sbushings, bearings and wear rings in pumps handling abrasive media up to 250°F (121°C). ARHT provides outs..
Compressive Strength 67.6 MPa
9800 psi
ASTM D695
ITW Devcon Metal Repair Wear Resistant Epoxy (WR-2), Dark Grey
Information provided by ITW Devcon
Compressive Strength 67.6 MPa
9800 psi
BCC Products BC 5200 Kwik-Set Adhesive
BC5200 is a medium viscosity fast gelling two part Epoxy Adhesive System. With an easy to use 1 to 1 mix ratio, BC5200 is considered an excellent general purpose adhesive for in-shop use. BC5200 wil..
Compressive Strength 67.6 MPa
9800 psi
BCC Products BC 8870 Polyurethane Elastomer
BC8870 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig..