Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 149 J | 110 ft-lb | |
Crucible Steel 304L Chromium-Nickel Steel Crucible 304L is a non-hardenable, low carbon austenitic chromium-nickel steel designed for special applications. It is particularly suitable for applications requiring welding operations where it i.. |