Polymer Property : Izod Impact Unnotched = 149 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 149 J
110 ft-lb
Crucible Steel 304L Chromium-Nickel Steel
Crucible 304L is a non-hardenable, low carbon austenitic chromium-nickel steel designed for special applications. It is particularly suitable for applications requiring welding operations where it i..