Mechanical Properties Metric English Comments
Izod Impact Unnotched 169 J
125 ft-lb
Oil Quenched from 1080°C
Latrobe DuraTechâ„¢ Xtreme Powder Metal Tool Steel
DuraTech Xtreme tool steel is a medium-carbon, powder metallurgy tool steel which has an outstanding combination of properties including very high impact toughness, very good hot hardness, and good ..