Latrobe DuraTechâ„¢ Xtreme Powder Metal Tool Steel

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , Medium Carbon Steel , Tool Steel
Manufacturer Latrobe Steel
Trade Name DuraTech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe DuraTechâ„¢ Xtreme Powder Metal Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuraTech Xtreme tool steel is a medium-carbon, powder metallurgy tool steel which has an outstanding combination of properties including very high impact toughness, very good hot hardness, and good wear resistance. The impact toughness is enhanced by the fine grain size, small carbides, and superior cleanliness of the powder metallurgy (PM) microstructure. Typically, when selecting a tool steel, one must choose between high strength or high toughness, with a compromise in the other of these two properties. However, with an attainable hardness in the low 60s Rockwell C, the unique properties of DuraTech Xtreme make it an excellent choice for tooling applications which require both high strength and high impact toughness, heat resistance, or all of the above. DuraTech Xtreme should be considered for the most extreme service in blanking dies, sizing dies, shear blades, cold and hot forging punches, forging dies, gear rolling dies, and many other applications where a combination of strength and toughnessTimken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.80 g/cc
7.80 g/cc
Density 7.81 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 61.5
61.5
Oil Quenched from 1066°C; 30 minutes
63.5
63.5
Oil Quenched from 1093°C; 15 minutes
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 65 - 70 %
65 - 70 %
1% Carbon Steel
Izod Impact Unnotched 94.9 J
70.0 ft-lb
Oil Quenched from 1080°C
169 J
125 ft-lb
Oil Quenched from 1080°C
Thermal Properties Metric English Comments
CTE, linear 11.97 µm/m-°C

@Temperature 38.0 - 427 °C
6.650 µin/in-°F

@Temperature 100 - 801 °F
12.71 µm/m-°C

@Temperature 38.0 - 649 °C
7.061 µin/in-°F

@Temperature 100 - 1200 °F
Component Elements Properties Metric English Comments
Carbon, C 0.55 %
0.55 %
Chromium, Cr 4.0 %
4.0 %
Iron, Fe 88.79 %
88.79 %
Manganese, Mn 0.40 %
0.40 %
Molybdenum, Mo 4.25 %
4.25 %
Nickel, Ni 0.50 %
0.50 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S 0.010 %
0.010 %
Vanadium, V 1.0 %
1.0 %