Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 29.8 J | 22.0 ft-lb | Oil Quenched at 1204°C; 538°C Temper Temperature |
Latrobe Crusaderâ„¢ ASTM M3-2 High Speed Steel CRUSADER (M3-2) is a high speed steel with an outstanding balance of red hardness, edge toughness and wear resistance. The additional carbon and vanadium provide good resistance to abrasion and edge.. |
|||
Izod Impact Unnotched | 29.8 J | 22.0 ft-lb | Oil Quenched at 1177°C; 520°C Temper Temperature |
Latrobe HS-29XLâ„¢ ASTM M2-HC High Speed Steel HS-29XL (M2-HC) is the M2 composition with the carbon content increased and with the addition of alloy sulfides. The higher carbon content provides higher hardness and
superior red hardness compared.. |
|||
Izod Impact Unnotched | 29.8 J | 22.0 ft-lb | Air Cooled from 1010°C; 483°C Temper Temperature |
Latrobe LSSâ„¢ D2 Tool Steel (ASTM D2) TLS D2 tool steel is a versatile high-carbon, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, large, chromium rich alloy carbides.. |
|||
Izod Impact Unnotched | 29.8 J | 22.0 ft-lb | For 63 HRC |
Latrobe LSSâ„¢ Vertex Tool Steel TLS Vertex tool steel is a versatile, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, chromium-rich alloy carbides in the micros.. |
|||
Izod Impact Unnotched | 29.8 J | 22.0 ft-lb | |
Carpenter Micro-Melt® 10 Wear Treated Tool Steel (AISI A11) Micro-Melt® 10 tool steel is a high vanadium tool steel produced using the Carpenter Micro-Melt powder process. This grade possesses wear resistance superior to most other tool steels along with go.. |