Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 67.8 J | 50.0 ft-lb | Air Cooled from 954°C; 94°C Temper Temperature |
Latrobe LSSâ„¢ A2 Tool Steel (ASTM A2) TLS A2 tool steel is a versatile, air-hardening tool steel that is characterized by good toughness and excellent dimensional stability in heat treatment. TLS A2 is intermediate in wear resistance be.. |
|||
Izod Impact Unnotched | 67.8 J | 50.0 ft-lb | Oil Quenched at 1121°C; 594°C Temper Temperature |
Latrobe CM-50â„¢ ASTM M50 High Speed Steel CM-50 is classified as an intermediate type high speed steel of the molybdenum chromium- vanadium variety. It is recommended for applications with moderate cutting conditions, such as woodworking to.. |
|||
Izod Impact Unnotched | 67.8 J | 50.0 ft-lb | |
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
Izod Impact Unnotched | 67.8 J | 50.0 ft-lb | |
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
Izod Impact Unnotched | 67.8 J | 50.0 ft-lb | when tempered around 1200°F |
Carpenter Hampden® High Carbon, High Chrome Tool Steel (Oil-Wear) (AISI D3) Hampden tool steel is an oil-hardening, high-carbon, high-chromium die steel having extreme wear resistance, It hardens with very little change in size or shape. Hampden tool steel is a deep-hardeni.. |