Material Notes:
TLS A2 tool steel is a versatile, air-hardening tool steel that is characterized by good toughness and excellent dimensional stability in heat treatment. TLS A2 is intermediate in wear resistance between O1 oil-hardening tool steel and D2 high-carbon, high-chromium tool steel. TLS A2 provides an effective combination of strength and toughness, tool performance, price, and a wide variety of product forms. Typical applications for TLS A2 tool steel include punches and dies, chuck jaws, cutting tools for woodworking, tooling for plastic injection, dowel pins, hammers, industrial knives, and gages.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.86 g/cc
7.86 g/cc
Density 7.86 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 63
63
Air Cooled from 982°C, 30 minutes
63.5
63.5
Air Cooled from 1038°C, 30 minutes
64
64
Air Cooled from 1010°C, 30 minutes
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 70 %
70 %
1% Carbon Steel
Izod Impact Unnotched 67.8 J
50.0 ft-lb
Air Cooled from 954°C; 94°C Temper Temperature
122 J
90.0 ft-lb
Air Cooled from 954°C; 316°C Temper Temperature
229 J
169 ft-lb
Air Cooled from 954°C; 649°C Temper Temperature
Thermal Properties Metric English Comments
CTE, linear 10.6 µm/m-°C

@Temperature 93.0 - 260 °C
5.89 µin/in-°F

@Temperature 199 - 500 °F
14.0 µm/m-°C

@Temperature 93.0 - 649 °C
7.78 µin/in-°F

@Temperature 199 - 1200 °F
Thermal Conductivity 26.001 W/m-K
180.44 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C 1.0 %
1.0 %
Chromium, Cr 5.0 %
5.0 %
Iron, Fe 91.7 %
91.7 %
Manganese, Mn 0.75 %
0.75 %
Molybdenum, Mo 1.0 %
1.0 %
Silicon, Si 0.30 %
0.30 %
Vanadium, V 0.25 %
0.25 %
Chemical Properties Metric English Comments
Critical Temperature 793 °C
1460 °F
Ac1