Polymer Property : Izod Impact Unnotched = 7.01 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 9.50 J
7.01 ft-lb
Kennametal Stellite Stellite® 12
Satisfactory finishing results can be obtained using carbide tipped tools. Applications include cutting plastics, rubber, paper, carpet, and wood; saw teeth, trimmer knives, carpet knives, ledger bl..