Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 10.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 10.0 J

@Temperature -20.0 °C
7.38 ft-lb

@Temperature -4.00 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem DT1800E PEI Blend
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re..
Impact Test 10.0 J

@Temperature -20.0 °C
7.38 ft-lb

@Temperature -4.00 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Asia Pacific)
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi..
Impact Test 10.0 J

@Temperature -20.0 °C
7.38 ft-lb

@Temperature -4.00 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Europe-Africa-Middle East)
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri..
Impact Test 10.0 J

@Temperature -30.0 °C
7.38 ft-lb

@Temperature -22.0 °F
ASTM D3763
Diamond Polymers Centrex® 810 Injection Molding Grade
Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and ..
Impact Test 10.0 J

@Thickness 4.00 mm
7.38 ft-lb

@Thickness 0.157 in
Multi-axial, at max. load; ASTM D3763
Azdel Plus C401-B01 40% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C401-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope..
Impact Test 10.0 J

@Thickness 4.00 mm
7.38 ft-lb

@Thickness 0.157 in
Multi-axial, at max. load; ASTM D3763
Azdel Plus C467-B01 45% Chopped Fiber Mat / PP Resin Matrix (Mineral filled)
AZDEL® C467-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu..
Impact Test 10.0 J

@Thickness 4.00 mm
7.38 ft-lb

@Thickness 0.157 in
Multi-axial, at max. load; ASTM D3763
Azdel Plus R300-B01 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R300-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr..
Impact Test 10.0 J

@Thickness 4.00 mm
7.38 ft-lb

@Thickness 0.157 in
Multi-axial, at max. force; ISO 6603-2
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia..
Impact Test 10.0 J

@Thickness 4.00 mm
7.38 ft-lb

@Thickness 0.157 in
Multi-axial, at max. force; ISO 6603-2
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Copyright © lookpolymers.com All Rights Reserved