Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 14.9 J @Temperature -17.8 °C |
11.0 ft-lb @Temperature 0.000 °F |
Multiaxial Impact, Driven Dart; 1/2" dart, 1-1/2" ring; E-tot; ASTM-D3763 |
Ineos ABS Lustran® Guardian™ 620 ABS, Extrusion Grade Lustran® Guardian™ ABS 620 is a high modulus, HFC 134a and HCFC 22 resistant extrusion grade resin designed for refrigerator door and food liners. Lustran® ABS 620 offers good melt streng.. |
|||
Impact Test | 14.9 J @Temperature 23.0 °C |
11.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 713.93 Molding, extrusion and compounding resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer with very good toughness, high clarity and excellent processability. It is suitable for use in making molded articles, extruded profile.. |
|||
Impact Test | 14.9 J @Temperature 23.0 °C |
11.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 755.12 Molding, extrusion and compounding resin Escorene Ultra LD 755.12 is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives.Availability: Latin America, North America and South America Additive: Antibl.. |
|||
Impact Test | 14.9 J @Temperature 23.0 °C |
11.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 755.CM Molding, extrusion and compounding resin Escorene Ultra LD 755.CM is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives.Availability: Latin America, North America and South America Additive: Antibl.. |
|||
Impact Test | 14.9 J @Temperature 23.0 °C |
11.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate OPTEMA TC 220 is an ethylene methyl acrylate copolymer, which can be used in specialty bonding applications and as a toughener for engineering polymers. It can been processed at temperatures as low .. |