Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 16.3 J @Temperature -40.0 °C |
12.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil OPTEMA™ TC 140 Molding, extrusion, compounding and adhesive resin
(discontinued **) OPTEMA TC 140 is a high flow, 21.5% methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compou.. |
|||
Impact Test | 16.3 J @Temperature 23.0 °C |
12.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 722.MV Molding, extrusion and compounding resin
(discontinued **) Escorene Ultra LD 722.MV is a high vinyl acetate copolymer resin for specialty extrusion and compounding application. Articles made from LD 722.MV are soft and have excellent low temperature toughne.. |
|||
Impact Test | 16.3 J @Temperature 23.0 °C |
12.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil Escorene® LD 767.MJ Molding, extrusion and compounding resin
(discontinued **) Escorene Ultra LD 767.MJ is a high viscosity, 29.5% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |
|||
Impact Test | 16.3 J @Temperature -17.8 °C |
12.0 ft-lb @Temperature 0.000 °F |
Multiaxial Impact, Total Energy; CEAST |
Ineos ABS Lustran® Guardian™ 732 ABS, Extrusion Grade Lustran® Guardian™ ABS 732 is an extrusion grade resin designed for use in thermoformed refrigerator and freezer liner applications. It is suitable for use with 245fa PU foams. |