Mechanical Properties Metric English Comments
Impact Test 20.3 J

@Temperature 23.0 °C
15.0 ft-lb

@Temperature 73.4 °F
Instrument Impact, Total Energy; ASTM D3763
ExxonMobil OPTEMA™ TC 115 Molding, extrusion and compounding resin  (discontinued **)
OPTEMA TC 115 is an ethylene methyl acrylate copolymer, which can be used as a compatibilizer and impact modifier for engineering thermoplastics. It has been processed at temperatures up to 625°F w..
Impact Test 20.3 J

@Temperature -40.0 °C
15.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy; ASTM D3763
ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate
OPTEMA TC 220 is an ethylene methyl acrylate copolymer, which can be used in specialty bonding applications and as a toughener for engineering polymers. It can been processed at temperatures as low ..
Impact Test 20.3 J

@Temperature 23.0 °C
15.0 ft-lb

@Temperature 73.4 °F
Multi-axial, at failure, measured on flat plaques; ASTM D3763
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (12 mm Molded Thickness)
AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..