Polymer Property : Impact Test = 21.9 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 21.9 J

@Temperature 22.8 °C
16.2 ft-lb

@Temperature 73.0 °F
Rheometric, 5mph, 1/2" diameter tup, 3" diameter ring
DuPont Bexloy® AXW507NC010 Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
Impact Test 21.9 J

@Temperature 22.8 °C
16.2 ft-lb

@Temperature 73.0 °F
Rheometric, 5mph, 1/2" diameter tup, 3" diameter ring
DuPont Bexloy® AXW504BK Modified Ionomer Resin  (discontinued **)
A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont.
Impact Test 21.9 J

@Temperature 22.8 °C
16.2 ft-lb

@Temperature 73.0 °F
Rheometric, 5mph, 1/2" diameter tup, 3" diameter ring
DuPont Bexloy® AXW602NC010 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin  (discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.
Impact Test 21.9 J

@Temperature 22.8 °C
16.2 ft-lb

@Temperature 73.0 °F
Rheometric, 5mph, 1/2" diameter tup, 3" diameter ring
DuPont Bexloy® AXW604BK 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin  (discontinued **)
A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont.